C-rate is the quickest way to compare a charge or discharge current across cells and packs of very different size. This calculator does the conversions in both directions: from a C-rate to amps, watts and time, or from a current, power or target time back to a C-rate, for a single cell or a full series-parallel pack. It is a companion to our C-rate definition page, which covers the background.

C-Rate, Current and Ah/Wh Calculator
Enter the capacity and voltage, then any one of C-rate, current, power or time. Everything else follows.
| C-rate | Pack current (A) | Power (kW) | Ideal time |
|---|
Ideal time is capacity divided by current. Real discharge time is shorter at high C-rate, because voltage sag and heating cut the usable capacity, and real charge time is longer because of the constant-voltage taper. Power is quoted at nominal voltage; at constant power the current rises as the voltage falls.
The Relationships
Everything in the calculator comes from four lines. Capacity and voltage scale with the pack configuration:
C-rate is the current divided by the capacity, and the ideal time is its inverse:
where Q is capacity (Ah), V is nominal voltage (V), E is energy (Wh), S and P are the number of cells in series and in parallel, I is current (A) and t is time in hours. When the input is a power, the calculator converts it to current at nominal voltage, I = W / Vpack, so the C-rate and the E-rate (power divided by energy) come out the same.
Worked Example
Take an illustrative LFP pack of 104 cells in series, each 100 Ah at 3.2 V nominal. That gives 332.8 V and 33.3 kWh. Asking it for 150 kW:
- Current at nominal voltage: 150,000 / 332.8 = 451 A
- C-rate: 451 / 100 = 4.5C
- Ideal time at that power: 60 / 4.5 = 13.3 minutes
A 4.5C continuous discharge is a demanding duty for a large prismatic LFP cell. The same 150 kW from a pack twice the capacity is 2.25C. That is why peak power, not energy, often sets the cell count in small packs.
Where the Simple Numbers Break Down
- Discharge at high C-rate. Ohmic and polarisation losses pull the terminal voltage down, so the cell reaches its lower cut-off before the rated capacity is delivered, and the extra heat adds its own limit. The ideal time is an upper bound. See Thermal Behaviour of the Li-Ion Cell for how continuous and peak ratings are set.
- Charging. A constant-current, constant-voltage charge spends its last part at falling current, so a 1C charge to 100% takes longer than the ideal hour. Fast-charge times are normally quoted for a partial window such as 10 to 80% for this reason.
- Constant power. At fixed power the current rises as the voltage falls through the discharge, so the C-rate at the bottom of the window is higher than at nominal voltage.
- Which capacity. Datasheets quote nominal capacity at a stated rate and temperature. Using a usable or end-of-life capacity instead raises the C-rate for the same current.
For quick sizing, the calculator is the right tool. For anything closer to the real pack, use cell test data such as HPPC pulse resistance and rate capability curves.
See also: C-rate, Thermal Behaviour of the Li-Ion Cell, Battery Calculators, Cell Heat Generation Calculator